甲烷在活性炭上裂解制氢研究

  • Received Date: 2005-05-27
  • Rev Recd Date: 2005-09-16
  • Publish Date: 2006-02-28
  • The hydrogen production by the direct thermal decomposition of natural gas is an promising approach for its nearly zero emission of COx and lower energy consumption compared to the traditional methane steam reforming. The activated carbon (AC) as the catalyst for methane decomposition has many advantages over the metal ones, such as low cost, rich supply and so on, while there is little literature reported on the detailed methane decomposition over ACs and the properties changes of the ACs. In this work, the hydrogen production from the methane decomposition over activated carbons was studied in a fixedbed quartztube reactor and at the same time the surface properties changes of the ACs including surface area, pore volume, micropore volume and pore distribution before and after use were analyzed. The results indicate that the methane decomposition over different ACs shows a similar behavior, i.e., the maximum methane conversion is reached in the initial stage and then gradually fallen down to a stable stage along with the reaction time, which shows that the mechanisms of methane decomposition over ACs are same. The deactivation of the AC catalysts is due to the carbon deposition produced by the methane decomposition, which corresponds to the weight gain of the deactivated AC catalysts. The methane conversion increases with the increase of temperature, residence time and the decrease of methane partial pressure. However, high temperature is unfavorable of the stability of ACs because of the too rapid reaction rate and the great amount of carbon deposition in the initial stage. The spent ACs after methane decomposition have lower surface area, pore and micropore volme, and larger pore diameter than those of fresh ones, which shows that the carbon deposition takes place in the pores especially in the micropores of ACs and leads to the block of the pores.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (1859) PDF downloads(1161) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return