Volume 35 Issue 04
Aug.  2007
Turn off MathJax
Article Contents
FU Maosheng, CHEN Linshen, LI Jianguo, CHEN Songying. 还原条件对NiFe2O4-δ结构稳定性及其催化分解CO2活性的影响[J]. Journal of Fuel Chemistry and Technology, 2007, 35(04): 431-435.
Citation: FU Maosheng, CHEN Linshen, LI Jianguo, CHEN Songying. 还原条件对NiFe2O4-δ结构稳定性及其催化分解CO2活性的影响[J]. Journal of Fuel Chemistry and Technology, 2007, 35(04): 431-435.

还原条件对NiFe2O4-δ结构稳定性及其催化分解CO2活性的影响

More Information
  • Corresponding author: FU Maosheng
  • Received Date: 2006-12-16
  • Rev Recd Date: 2007-04-03
  • Publish Date: 2007-08-30
  • Nickel ferrite, NiFe2O4, with spinel structure was prepared by citrate coordination method. The samples were characterized by X-ray diffraction (XRD) thermal gravimetric analysis (TGA). When the weight of NiFe2O4 sample was 0.5g, the optimum reduction condition for the preparation of oxygendeficient nickel ferrite, NiFe2O4-δ, reduced by H2 was as follows: reduction temperature was 320℃, H2 flow rate was 40mL/min and reduction time was 3h. The results also showed that the higher reduction temperature and higher H2 flow rate as well as longer reduction time led to an excessive reduction of NiFe2O4-δ and the destructiveness of its spinel structure, resulting in the formation of FeNi alloy Fe(Ni) as well as α-Fe phase.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (1882) PDF downloads(469) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return